China LLDPE Film Extrusion Linear Low Density Polyethylene Pellets Petrothene GA501

LLDPE Film Extrusion Linear Low Density Polyethylene Pellets Petrothene GA501

Density (23°C): 0.918 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 1 G/10 Min
Processing Method: Film Extrusion
China Prime Polymer Evolue Sp3010 Blown Film

Prime Polymer Evolue Sp3010 Blown Film

Melt Mass-Flow Rate (MFR): 0.8 G/10 Min
Density: 0.926 G/cm³
Processing Method: Blown Film
China Prime Polymer Evolue Sp2120

Prime Polymer Evolue Sp2120

Melt Mass-Flow Rate (MFR): 2.2 G/10 Min
Density: 0.921 G/cm³
Processing Method: Blown Film
China Polyethylene LLDPE Granules Bio Based Sugarcane Braskem Green PE SLL318

Polyethylene LLDPE Granules Bio Based Sugarcane Braskem Green PE SLL318

Density (23°C): 0.918 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 2.7 G/10 Min
Molding Temperature: 170 -180 °C
China Bio Based Sugarcane LLDPE Polyethylene Granules Braskem Green PE SLL118/21

Bio Based Sugarcane LLDPE Polyethylene Granules Braskem Green PE SLL118/21

Density (23°C): 0.918 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 1 G/10 Min
Processing Method: Blown Film ,Film Extrusion
China Braskem Green PE SLL118 Bio Based Sugarcane Polyethylene LLDPE Plastic Granules

Braskem Green PE SLL118 Bio Based Sugarcane Polyethylene LLDPE Plastic Granules

Density (23°C): 0.916 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 1 G/10 Min
Processing Method: Blown Film Extrusion.
China Bio Based Sugarcane Polyethylene LLDPE Granules Braskem Green PE SLH218

Bio Based Sugarcane Polyethylene LLDPE Granules Braskem Green PE SLH218

Density (23°C): 0.916 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 2.3 G/10 Min
Processing Method: Blown Film Extrusion.
China Prime Polymer Evolue SP2040 Cast Film Mlldpe

Prime Polymer Evolue SP2040 Cast Film Mlldpe

Melt Mass-Flow Rate (MFR): 3.8 G/10 Min
Density: 0.918 G/cm³
Processing Method: Cast Film
China Prime Polymer Evolue SP1540 Cast Film Mlldpe

Prime Polymer Evolue SP1540 Cast Film Mlldpe

Melt Mass-Flow Rate (MFR): 3.8 G/10 Min
Density: 0.913 G/cm³
Processing Method: Cast Film
China Bio Based Sugarcane LLDPE Linear Low Density Polyethylene Granules Braskem LH0820/30AF

Bio Based Sugarcane LLDPE Linear Low Density Polyethylene Granules Braskem LH0820/30AF

Density (23°C): 0.918 G/cm³
Melt Mass-Flow Rate (MFR) (190°C/2.16 Kg): 0.8 G/10 Min
Processing Method: Blown Film ,Film Extrusion