VIDEO Good price Chimei Polylac PA-746 High Flow High Impact Resistance ABS Granules online

Chimei Polylac PA-746 High Flow High Impact Resistance ABS Granules

Processing Temperature: 200-250°C
Impact Strength: 3-5 KJ/m2
Uv Resistance: Good
Good price Prime Polymer Evolue Sp2020 Lldpe Blown Film online

Prime Polymer Evolue Sp2020 Lldpe Blown Film

Melt Mass-Flow Rate (MFR): 2.3 G/10 Min
Density: 0.916 G/cm³
Processing Method: Blown Film
Good price Prime Polymer Evolue Sp1510 Lldpe, Blown Film online

Prime Polymer Evolue Sp1510 Lldpe, Blown Film

Melt Mass-Flow Rate (MFR): 1.0 G/10 Min
Density: 0.915 G/cm³
Durometer Hardness (Shore D, Injection Molded): 55
Good price Prime Polymer Evolue PE SP4020 Blown Film online

Prime Polymer Evolue PE SP4020 Blown Film

Melt Mass-Flow Rate (MFR): 1.8 G/10 Min
Density: 0.937 G/cm³
Processing Method: Blown Film
Good price Prime Polymer Evolue PE SP2520 Blown Film online

Prime Polymer Evolue PE SP2520 Blown Film

Melt Mass-Flow Rate (MFR): 1.9 G/10 Min
Density: 0.925 G/cm³
Processing Method: Blown Film
Good price Prime Polymer Evolue PE SP2320 Blown Film online

Prime Polymer Evolue PE SP2320 Blown Film

Melt Mass-Flow Rate (MFR): 1.9 G/10 Min
Density: 0.92 G/cm³
Processing Method: Blown Film
Good price Prime Polymer Evolue Sp1520  Blown Film online

Prime Polymer Evolue Sp1520 Blown Film

Melt Mass-Flow Rate (MFR): 2 G/10 Min
Density: 0.919 G/cm³
Durometer Hardness (Shore D, Injection Molded): 54
Good price Prime Polymer Evolue Sp0510 Lldpe Blown Film online

Prime Polymer Evolue Sp0510 Lldpe Blown Film

Melt Mass-Flow Rate (MFR): 1.2 G/10 Min
Density: 0.903 G/cm³
Durometer Hardness (Shore D, Injection Molded): 50
Good price Petrothene® NA480178 LyondellBasell LDPE online

Petrothene® NA480178 LyondellBasell LDPE

Density: 0.923 G/cm³
Melt Flow Rate (MFR) (190°C/2.16 Kg): 0.25 G/10 Min
Processing Methods: Extrusion, Blown Film
Good price Petrothene® NA480145 LyondellBasell LDPE online

Petrothene® NA480145 LyondellBasell LDPE

Density: 0.923 G/cm³
Melt Flow Rate (MFR) (190°C/2.16 Kg): 0.25 G/10 Min
Processing Methods: Extrusion, Blown Film